This paper discusses the effect of some important parameters on cyclic behavior of sub-substandard interior beam-column connection. The objective is to investigate the effect of joint shear stress, anchorage bond of longitudinal beam bar within the joint and horizontal joint reinforcements on the joint performance. The experiment consisted of five half-scale beam-column specimens. The control specimen (J1) represented a typical non-ductile beam-column joint in mid-rise RC buildings constructed in low seismic zone. In specimen J2, the bond between concrete and longitudinal bars was completely removed initially. In specimen J3A and J3B, a substantial amount of horizontal joint reinforcement was provided in joint core. In specimen J4, the column size was enlarged to reduce shear stress in joint. The experimental result demonstrated brittle joint shear failure in control specimen (J1), specimens J3A and J3B, beam splitting failure in specimen J2 and ductile flexural failure in specimen J4. Based on experimental results, it was found that the initial lost of bond did not cause a substantial reduction in joint capacity. Moreover, provision of substantial horizontal joint reinforcements in specimen J3A and J3B did not produce a comparable improvement in the seismic performance. With increased column size in specimen J4, the energy dissipation characteristics were greatly improved as indicated by large spindle-shaped cyclic loops.
机译:本文讨论了一些重要参数对次标准内部梁柱连接的循环行为的影响。目的是研究接缝剪应力,接缝内纵梁的锚固结合以及水平接缝钢筋对接缝性能的影响。实验由五个半比例的梁柱标本组成。对照样本(J1)代表了在低地震带中建造的中层RC建筑物中的典型非延性梁柱节点。在试样J2中,混凝土和纵向钢筋之间的粘结首先被完全去除。在试样J3A和J3B中,在接头芯中提供了大量的水平接头加固。在试样J4中,扩大了柱的尺寸以减小接头的剪切应力。实验结果表明,在控制试样(J1),试样J3A和J3B中,脆性接头剪切破坏,试样J2中的光束分裂破坏和试样J4中的延性挠曲破坏。根据实验结果,发现最初的结合力损失并没有引起结合能力的大幅降低。此外,在试样J3A和J3B中提供大量的水平缝补强并没有在地震性能方面产生可比的改善。随着标本J4中柱尺寸的增加,能量消耗特性得到了极大的改善,如大型主轴形循环回路所示。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号