Poly(3-hydroxybutyrate)ano-hydroxyapatite (PHBHA) composite scaffolds were fabricated without the use of organic solvents at different mass fractions of HA nanopartides. HA nanopartides were homogeneously dispersed as primary particles in the polymer matrix of the scaffolds at 10 and 15 wt.% nHA content. Agglomeration of HA nanopartides occurred when the nHA content of the scaffolds reached 20 wt.%. All the scaffolds had high porosities with interconnected porous structure and optimized pore size ranges. Mechanical properties of all the scaffolds were in the range of mechanical properties of cancellous bone. Scaffolds were biocompatible to MG-63 cells in the indirect method of cytotoxicity evaluation. Also, the morphology of the attached MG-63 cells in direct contact with the scaffolds indicated the appropriate cell-scaffold interaction. Thus, the PHBHA composite scaffolds investigated in this study tend to be favorable for bone tissue engineering applications.
机译:在不使用有机溶剂的情况下,在HA纳米粒子的不同质量分数下,制备了聚(3-羟基丁酸酯)/纳米羟基磷灰石(PHB / nHA)复合支架。 HA纳米颗粒作为初级颗粒以nHA含量为10和15 wt%的形式均匀分散在支架的聚合物基质中。当支架的nHA含量达到20 wt。%时,会发生HA纳米颗粒的团聚。所有的支架都具有高孔隙率,相互连接的多孔结构和最佳的孔径范围。所有支架的机械性能都在松质骨的机械性能范围内。在间接的细胞毒性评估方法中,支架与MG-63细胞具有生物相容性。而且,附着的MG-63细胞与支架直接接触的形态表明适当的细胞-支架相互作用。因此,在这项研究中研究的PHB / nHA复合支架倾向于对骨组织工程应用有利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号