'Cotton-ball' shaped porous iron-nickel sulfide: A high-rate cathode for long-life aqueous rechargeable battery

机译:'棉球'形多孔铁 - 硫化镍:长寿命水性可充电电池的高速阴极

获取原文
获取原文并翻译 | 示例
           

摘要

Aqueous rechargeable batteries (ARB) offer reasonably higher energy density and cycle life than their nonaqueous counterparts. Yet, the bottleneck is a limited choice of positive electrodes coupled with low-rate capability and inadequate cycle life. We report here a wet chemical approach to synthesize in-situ three-dimensional (3D) 'cotton-ball' shaped porous iron-nickel sulfide (FeNi2S4) (henceforth referred to as PINS) as a diffusion-controlled ARB electrode. It shows a high specific capacity of 177 mA h g(-1) at 1 A g(-1) vs Pt in the alkaline electrolyte with excellent rate capability (89 mA h g(-1) at 40 A g(-1)) and ultra-long cycle life (10,000 cycles). Furthermore, a pouch-type full-cell ARB (FeNi2S4//AC) delivers an energy density of 56.7 Wh kg(-1) at a power density of 871.5 W kg(-1) with high cycling stability (10,000 cycles). The present study offers a straightforward and efficient approach for developing nanostructured transition metal sulfide-based cathode materials for practical ARB.
机译:含水可充电电池(ARB)提供比其非水对应物更高的能量密度和循环寿命。然而,瓶颈是具有低速率能力和循环寿命不足的正电极的有限选择。我们在此报告一种湿化学方法,用于合成原位三维(3D)'棉球'形多孔铁 - 硫化镍(FENI2S4)(以下称为引脚)作为扩散控制的ARB电极。它在碱性电解质中以1Ag(-1)Vs Pt在碱性电解质中为1Ag(-1)Vs Pt的高比容量,具有优异的速率能力(89mA Hg(-1),40Ag(-1))和超长循环寿命(10,000个循环)。此外,袋式全细胞arb(Feni2s4 // AC)以高循环稳定性(10,000个循环)的功率密度以871.5Wkg(-1)的功率密度提供56.7WHKG(-1)的能量密度。本研究提供了一种直接和有效的方法,用于开发用于实际坯的纳米结构过渡金属硫化物的阴极材料。

著录项

  • 来源
    《Materials Research Bulletin》 |2021年第8期|111307.1-111307.11|共11页
  • 作者单位

    CSIR Cent Glass & Ceram Res Inst 196 Raja SC Mullick Rd Kolkata 700032 India|Univ St Andrews Sch Chem Purdie Bldg North Haugh St Andrews Fife Scotland;

    CSIR Cent Glass & Ceram Res Inst 196 Raja SC Mullick Rd Kolkata 700032 India|Bar Ilan Univ Dept Chem Ramat Gan Israel;

    CSIR Cent Glass & Ceram Res Inst 196 Raja SC Mullick Rd Kolkata 700032 India|Univ St Andrews Sch Chem Purdie Bldg North Haugh St Andrews Fife Scotland;

    CSIR Cent Glass & Ceram Res Inst 196 Raja SC Mullick Rd Kolkata 700032 India|SN Bose Natl Ctr Basic Sci Kolkata India;

    CSIR Cent Glass & Ceram Res Inst 196 Raja SC Mullick Rd Kolkata 700032 India;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);美国《生物学医学文摘》(MEDLINE);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Ternary metal sulfide; FeNi2S4; Hydrothermal synthesis; Aqueous rechargeable battery; Electrochemical energy storage;

    机译:三元金属硫化物;FENI2S4;水热合成;水性可充电电池;电化学储能;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号