This paper reports the effect of post weld heat treatment on fatigue behaviour of electron beam welded AA2219 aluminium alloy. An attempt has been made to enhance the fatigue strength of the electron beam welded joints through post weld heat treatment methods such as solution treatment, artificial aging, solution treatment and artificial aging. Electron beam welding machine with 100 kV capacity has been used to fabricate the square butt joints. Servo hydraulic controlled fatigue testing machine with a capacity of 100 kN has been used to evaluate the fatigue life of the welded joints. Of the three post weld heat treated joints, the solution treated and aged joints are enduring higher number of cycles under the action of cyclic loads.
机译:本文报道了焊后热处理对电子束焊接AA2219铝合金疲劳行为的影响。已经尝试通过焊后热处理方法,例如固溶处理,人工时效,固溶处理和人工时效来增强电子束焊接接头的疲劳强度。具有100 kV容量的电子束焊接机已用于制造方形对接接头。容量为100 kN的伺服液压控制疲劳试验机已用于评估焊接接头的疲劳寿命。在三个焊后热处理接头中,固溶处理和时效接头在循环载荷的作用下承受着更高的循环次数。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号