This paper attempts to investigate the influence of the microstructural changes on the dry sliding wear behaviour of Al-12Si and Al-12Si-3Cu cast alloys by grain refinement (Al-1Ti-3B), modification (Al-10Sr) and combined action of both (Al-1Ti-3B + Al-10Sr). Results indicate that combined grain refined and modified Al-12Si-3Cu cast alloys have microstructures consisting of uniformly distributed (α-Al grains, eutectic Al-silicon and fine CuAl_2 particles in the interdendritic region. These alloys exhibited better wear resistance in the cast condition compared with the same alloy subjected to only grain refinement or modification. The improved wear resistances of Al-12Si-3Cu cast alloys are related to the refinement of the aluminum grain size, uniform distribution of eutectic Al-silicon and fine CuAl_2 particles in the interdendritic region resulting from combined refinement and modification.
机译:本文试图通过晶粒细化(Al-1Ti-3B),变质(Al-10Sr)和铝的组合作用研究微观组织变化对Al-12Si和Al-12Si-3Cu铸造合金的干滑动磨损行为的影响。两者(Al-1Ti-3B + Al-10Sr)。结果表明,晶粒细化和改性后的Al-12Si-3Cu铸造合金的显微组织由均匀分布的(α-Al晶粒,共晶Al-硅和细小的CuAl_2颗粒组成)在枝晶间区域,这些合金在铸造条件下表现出更好的耐磨性与仅进行晶粒细化或改性的相同合金相比,Al-12Si-3Cu铸造合金耐磨性的提高与铝晶粒尺寸的细化,共晶Al-Si的均匀分布以及细小的CuAl_2颗粒在枝晶间的分布有关。细化和修改相结合产生的区域。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号