Under heavy loading and large numbers of revolutions, the most commonly encountered gear damage is the thermal damage that is caused by an accumulation of heat on the surface of the tooth. The maximum Hertzian surface stress occurs at the single tooth pair contact region. The aim of this study was to delay the formation of thermal damage in the region of single tooth meshing by decreasing the Hertzian surface pressure by increasing the tooth width. The F/b (N/mm) tooth load was decreased in the single tooth pair contact region. Experiments show that the appearance of thermal damage is delayed for the width-modified gear teeth in comparison with unmodified gear teeth.
机译:在重负载和大转数下,最常见的齿轮损坏是由于热量在牙齿表面积聚而引起的热损坏。最大的赫兹表面应力发生在单齿对接触区域。这项研究的目的是通过增加齿宽来降低赫兹表面压力,从而延迟单齿啮合区域热损伤的形成。在单齿对接触区域中,F / b(N / mm)齿负荷减小。实验表明,与未修改的齿轮相比,宽度修改的齿轮的热损伤出现有所延迟。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号