The paper describes an experimental research on fracture characteristics of self-compacting concrete (SCC). Three point bending tests conducted on 154 notched beams with different water to cement (w/ c) ratios. The specimens were made from mixes with various w/c ratios from 0.7 to 0.35. For all mixes, common fracture parameters were determined using two different methods, the work-of-fracture method (WFM) and the size effect method (SEM). Test results showed that with decrease of w/c ratio from 0.7 to 0.35 in SCC: (a) the fracture toughness increases linearly: (b) the brittleness number is approximately doubled: (c) the effective size of the process zone c_f in SEM and the characteristic length (l_(ch)) in WFM decrease which may be explained by the change in structural porosity of the aggregate-paste transition zone; and (d) the fracture surface of concrete is roughly smoother, which can be attributed to the improved bond strength between the aggregates and the paste. Also, the results showed that there is a correlation between the fracture energy measured by WFM (G_F) and the value measured through SEM (G_f) (G_f ≌ 2.92G_f).
机译:本文描述了自密实混凝土(SCC)断裂特性的实验研究。在154个带不同水灰比(w / c)的带槽梁上进行了三点弯曲测试。样品由w / c比率从0.7到0.35的混合物制成。对于所有混合物,使用两种不同的方法(断裂功法(WFM)和尺寸效应法(SEM))确定共同的断裂参数。测试结果表明,随着SCC中w / c比从0.7降低到0.35:(a)断裂韧性线性增加:(b)脆性值近似加倍:(c)SEM中加工区c_f的有效尺寸WFM的特征长度(l_(ch))减小,这可以用骨料-浆体过渡区的结构孔隙率变化来解释。 (d)混凝土的断裂表面大致较光滑,这可以归因于骨料与浆体之间的粘结强度提高。此外,结果表明,通过WFM(G_F)测量的断裂能与通过SEM(G_f)测量的断裂能之间存在相关性(G_f≌2.92G_f)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号