机译:成形参数对Ti-6Al-4V电子束Surfi-Sculpt突起的影响
Science and Technology on Power Beam Processes Laboratory, Beijing Aeronautical Manufacturing Technology Research Institute, Beijing 100024, China,Department of Mechanical Engineering, Imperial College London, London SW7 2AZ, UK,Huazhong University of Science and Technology, Wuhan 430074, China;
Department of Mechanical Engineering, Imperial College London, London SW7 2AZ, UK;
Department of Mechanical Engineering, Imperial College London, London SW7 2AZ, UK;
Department of Materials, Imperial College London, London SW7 2AZ, UK;
Department of Mechanical Engineering, Imperial College London, London SW7 2AZ, UK;
Titanium alloy; Electron beam method; Protrusion; Microstructure; Hardness test;
机译:基于磁场控制的电子束造型技术研究
机译:基于α-Ti的Ti-6Al-4V合金的α-Ti对固体束处理的α-Ti的相位成分和晶格参数的变化
机译:选择性电子束熔化Ti-6Al-4V合金的微观结构,孔隙率,力学性能和构建模式参数之间的微观关系
机译:在Ti-6Al-4V合金上的电子束冲浪〜(Tm)期间的形成过程
机译:电子束后处理熔化Ti-6Al-4V和粘合剂喷射17-4不锈钢
机译:制备参数对电子束熔炼Ti-6Al-4V钛合金的组织和吸氢行为的影响
机译:形成参数对Ti-6al-4V电子束surfi-sculpt凸起的影响