Effect of pulse frequency on microstructure and properties of welded joints for dual phase steel by pulsed laser welding

机译:脉冲频率对脉冲激光焊接双相钢焊接接头组织和性能的影响

获取原文
获取原文并翻译 | 示例
           

摘要

This paper investigated the metallurgical phenomena of overlapping zone between two laser spots and related effects of pulse frequency (3-15 Hz) on properties of welded joints by pulsed laser welding for DP 590 steel sheets. The welded surfaces were not continuous at 3 and 5 Hz and shallow penetrations, but welded joints with full penetration were obtained at 8-15 Hz, caused by increasing average power. The microstructure evolution of fusion zone (FZ) with pulse frequency increasing was: lath martensite. lath martensite and bainite -> bainite and grain boundary ferrite. When pulse frequency was 3-8 Hz, overlapping zone was divided into four areas (FZ of former spot, super-critically HAZ (SC-HAZ), inter-critically HAZ (IC-HAZ), sub-critically HAZ (S-CHAZ)) wherein the microstructure changed with the increase of heat input. Hardness distribution of welded surface (3-8 Hz) was in zig-zag pattern and hardness dropped in S-CHAZ and IC-HAZ owing to the different microstructures. An increasing pulse frequency led to a hardness decrease in the cross-sectional of welded joints. For the full penetration of welded joints, tensile test revealed that strength of FZ was superior compared with base metal, and Erichsen value of welded joints could reach to 80% of the base metal when pulse frequency increased to 10-15 Hz. (C) 2016 Elsevier Ltd. All rights reserved.
机译:本文研究了DP 590钢板在两个激光点之间重叠区域的冶金现象以及脉冲频率(3-15 Hz)对脉冲激光焊接接头性能的相关影响。焊接表面在3和5 Hz时不连续,熔深较浅,但由于平均功率增加,在8-15 Hz时获得了全熔透的焊接接头。随着脉冲频率的增加,熔合区(FZ)的组织演变为:板条马氏体。板条马氏体和贝氏体->贝氏体和晶界铁素体。当脉冲频率为3-8 Hz时,重叠区域分为四个区域(原点的FZ,超临界HAZ(SC-HAZ),临界间HAZ(IC-HAZ),次临界HAZ(S-CHAZ) )),其中微观结构随热量输入的增加而变化。焊接表面的硬度分布(3-8 Hz)呈锯齿形,由于显微组织不同,S-CHAZ和IC-HAZ的硬度下降。脉冲频率的增加导致焊接接头横截面的硬度降低。对于焊接接头的完全渗透,拉伸试验表明,FZ的强度优于母材,当脉冲频率增加到10-15 Hz时,焊接接头的Erichsen值可达到母材的80%。 (C)2016 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号