Metakaolin geopolymer bricks (MKGB) were synthesised in this investigation with different percentages of flyash (FA) and Metakaolin (MK). A desired strength of 5.5 N/mm~2is achieved by using 50% FA and 50% MK. The bricks were tested for properties like water absorption, initial rate of absorption, efflorescence, modulus of elasticity (MOE) and modular ratio. Initial rate of absorption for the MKGB is 0.5 Kg/m~2/min and the water absorption for MKGB is 3-5%. The Poisson's ratio (μ) for MKGB is 0.2 and E is 2340 MPa. Metakaolin Geopolymer brick prisms (MKBP) with aspect ratios ranging between 2-5 were constructed with 1:3 cement mortar. The compressive strength and the efficiency increases with the increase in aspect ratio of the masonry. The failure pattern is splitting and crushing of bricks rather than loss of bond between mortar and MKGB.
机译:在该调查中合成了Metakaolin Geo聚物砖(MKGB),用不同百分比的Flyash(Fa)和Metakaolin(MK)。通过使用50%Fa和50%MK实现的所需强度为5.5n / mm〜2。测试砖的性质,如吸水性,初始吸收率,开花,弹性模量(MOE)和模块化比例。 MKGB的初始吸收率为0.5kg / m〜2 / min,MKGB的吸水率为3-5%。 MKGB的泊松比(μ)为0.2,e是2340MPa。具有2-5之间的偏塔林地缘聚合物砖棱镜(MKBP)在2-5之间,用1:3水泥砂浆构建。随着砌体的纵横比的增加,抗压强度和效率增加。故障模式是分裂和粉碎砖而不是砂浆和MKGB之间的粘合。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号