La_(1.3-x)Sm_xCaMg_(0.7)Ni_9 (x=0-0.3) hydrogen storage alloys were prepared by inductive melting and the effect of the Sm content on the structure and electrochemical properties was investigated in the paper. The Sm substitution for La in La_(1.3-x)Sm_xCaMg_(0.7)Ni_9 (x = 0-0.3) alloys does not change the main phase structure (the rhombohedral PuNi_3-type structure), but leads to a shrinkage of unit cell and a decrease of hydrogen storage capacity. With the increase of the Sm content in the alloys, the maximum discharge capacity of electrode decreases from 400.2 (x=0) to 346.6 mAh g~(-1) (x = 0.3), but the high-rate dischargeability and cycling stability is improved. After 100 cycles, the capacity retention rate increases from 75 (x = 0) to 85% (x = 0.3).
机译:通过感应熔化制备了La_(1.3-x)Sm_xCaMg_(0.7)Ni_9(x = 0-0.3)储氢​​合金,并研究了Sm含量对结构和电化学性能的影响。 La_(1.3-x)Sm_xCaMg_(0.7)Ni_9(x = 0-0.3)合金中La的Sm替代不会改变主相结构(菱形PuNi_3型结构),但会导致晶胞收缩和储氢能力下降。随着合金中Sm含量的增加,电极的最大放电容量从400.2(x = 0)降低到346.6 mAh g〜(-1)(x = 0.3),但高倍率放电性能和循环稳定性却达到了改善。 100个周期后,容量保留率从75(x = 0)增加到85%(x = 0.3)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号