Long term testing of start-stop cycles on high temperature PEM fuel cell stack

机译:高温PEM燃料电池堆起停循环的长期测试

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

A PEM fuel cell with an operating temperature above 100 ℃ is desired for increasing the kinetics of reactions, reduced sensitivity to impurities of the fuel, as well as for the reduction of the requirements on thermal and water management systems. High Temperature Polymer Electrolyte Membrane Fuel Cells (HT-PEMFC) can effectively be combined with CHP systems to offer a simple system design and higher overall system efficiencies. For HT-PEMFC systems, the development of elaborated start/stop strategies is essential in mitigation of fuel cell degradation during these events. A 5 cell co-flow stack is assembled with BASF P1100W membrane electrode assembly (MEA) with an active area of 163.5 cm~2. Continuous operation and more than 1500 start stop cycles have been performed in order to study the degradation effects of both continuous operation and of repeated start stops using a protective start-stop algorithm, which is designed to avoid the formation of aggressive cell potentials. The repeated use of this procedure led to a degradation of 26 μV/cycle at a current density of 0.25 A cm~(-2) and 11 μV/cycle at a current density of 0.03 A cm~(-2). At open circuit voltage (OCV), a higher degradation rate of 133 μV/cycle was observed.
机译:为了提高反应动力学,降低对燃料杂质的敏感性以及降低对热和水管理系统的要求,需要工作温度高于100℃的PEM燃料电池。高温聚合物电解质膜燃料电池(HT-PEMFC)可以有效地与CHP系统结合使用,以提供简单的系统设计和更高的整体系统效率。对于HT-PEMFC系统,制定详细的启动/停止策略对于缓解这些事件期间燃料电池的退化至关重要。 5单元同流堆栈与BASF P1100W膜电极组件(MEA)组装在一起,有效面积为163.5 cm〜2。为了研究连续运行和重复启动停止的退化效果,已经进行了连续运行和超过1500个启动停止循环,这是采用保护性启动停止算法进行的,该算法旨在避免形成激进的细胞电势。重复使用此程序会导致在0.25 A cm〜(-2)的电流密度下降低26μV/周,在0.03 A cm〜(-2)的电流密度下降低11μV/周。在开路电压(OCV)下,观察到更高的降解速率133μV/周期。

著录项

  • 来源
    《Journal of power sources》 |2015年第1期|312-316|共5页
  • 作者单位

    Zentrum fuer Sonnenenergie- und Wasserstoff-Forschung Baden-Wuerttemberg (ZSW), Helmholtzstr. 8, 89081 Ulm, Germany;

    Zentrum fuer Sonnenenergie- und Wasserstoff-Forschung Baden-Wuerttemberg (ZSW), Helmholtzstr. 8, 89081 Ulm, Germany;

    Zentrum fuer Sonnenenergie- und Wasserstoff-Forschung Baden-Wuerttemberg (ZSW), Helmholtzstr. 8, 89081 Ulm, Germany;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);美国《生物学医学文摘》(MEDLINE);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    High temperature PEM fuel cell; PBI/H_3PO_4; Performance degradation; Start-stop; Long term testing;

    机译:高温PEM燃料电池;PBI / H_3PO_4;性能下降;启停长期测试;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号