首页> 外文期刊>Journal of Materials Science. Materials in Medicine >In vitro microhardness of glass ionomer cements
【24h】

In vitro microhardness of glass ionomer cements

机译:玻璃离聚物水泥的体外显微硬度

获取原文
获取原文并翻译 | 示例
           

摘要

This study evaluated the surface microhardness of four glass ionomer cements and a composite resin (Fuji IX, Ketac Molar, Vidrion R, Vitromolar and Z 250). Ten specimens of each glass ionomer cement with 8.0 mm diameter and 5.0 mm high dimensions were made and Vicker's micro-hardness measurements were taken at 1 day and 1 week after initial setting reaction. The results were analyzed using Student's T test and Tukey test (p < 0.05) and demonstrated that the values of microhardness increased after 1 week, with the exception of Fuji IX. Resin composite Z250 presented the greatest values for microhardness.
机译:这项研究评估了四种玻璃离聚物水泥和复合树脂(Fuji IX,Ketac Molar,Vidrion R,Vitromolar和Z 250)的表面显微硬度。每种直径为8.0 mm,高尺寸为5.0 mm的玻璃离聚物水泥分别制成10个样品,并在初始固化反应后1天和1周进行维氏显微硬度测量。使用Student's T检验和Tukey检验(p <0.05)对结果进行了分析,结果表明,除了Fuji IX外,显微硬度值在1周后有所增加。树脂复合材料Z250具有最高的显微硬度值。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号