New Evaluation on the Preoxidation Extent of Different PAN Precursors

机译:不同PAN前驱体预氧化程度的新评价。

获取原文
获取原文并翻译 | 示例
           

摘要

Structural changes in carbon fibers at each stage of, especially, preoxidation process are well known to play a great role in achieving the ultimate product quality. Differential scanning calorimetry (DSC), scanning electron microscope (SEM), density method and optical microscope were used to characterize the preoxidation extent. A conventional approach, e.g., density aim, to evaluate the extent of preoxidation is not very exact. A DSC curve of a PAN precursor only can provide general information, major in the temperature regime of preoxidation reaction. However, the evaluation of a preoxidation extent, especially from conventional preoxidation temperature with a great span regime of 200 approx 400 deg C, is put forward in this paper, in which the evolution of core/shell morphological structure is a kind of straightforward evidence.
机译:众所周知,碳纤维在预氧化过程的每个阶段的结构变化在实现最终产品质量方面都起着重要作用。用差示扫描量热法(DSC),扫描电子显微镜(SEM),密度法和光学显微镜表征了预氧化程度。诸如密度目标的常规方法来评估预氧化程度不是很精确。 PAN前体的DSC曲线只能提供一般信息,主要是预氧化反应的温度范围。然而,本文提出了对预氧化程度的评估,特别是从常规的预氧化温度,在200到400℃左右的大跨度范围内进行评估,其中核/壳形态结构的演变是一种直接的证据。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号