The present study aims to quantify the fatigue characteristics of nanoclay-modified binders, considering different analysis procedures in the linear amplitude sweep (LAS) test. Four unmodified and modified asphalt binders were subjected to the LAS test at 10°C, 20°C, and 30°C. The fatigue life obtained using five different analytical methods were assessed and compared. The effect of controlled strain rate (CSR) used in the LAS test was not found to be significant in changing the fatigue ranking of asphalt binders. Different analytical methods produce different fatigue curves with no change in the relative ranking of the binders at each temperature. The model parameters (a and b) obtained by fitting the relationship between average released pseudostrain energy (G~R) and the number of cycles to failure (N_f) can significantly impact fatigue life, resulting in a discrepancy in the results. This discrepancy, across different temperatures and binder types, can be removed by smoothening of the model with b = -2. The unified G~R-R-based analysis, as is proposed in this study, results in a lower value of fatigue life at lower strain susceptibility in the standard fatigue model. Statistical analysis reveals that there is no distinct influence of nanoclay on the fatigue life of asphalt binders. Inclusion of nanoclay results in either similar or marginally higher fatigue life at all the temperatures. The analysis and results support the use of a G~R-R-based approach for quantifying the fatigue life of asphalt binders.
机译:本研究旨在量化纳米粘土改性粘合剂的疲劳特性,考虑到线性振幅扫描(LAS)测试中的不同分析程序。在10℃,20℃和30℃下进行四种未改性和改性的沥青粘合剂。评估和比较使用五种不同分析方法获得的疲劳寿命。在改变沥青粘合剂的疲劳排名方面,未发现LAS测试中使用的受控菌株(CSR)的影响是显着的。不同的分析方法产生不同的疲劳曲线,每个温度下粘合剂的相对排名没有变化。通过拟合平均释放的伪杆菌能量(G〜R)之间的关系获得的模型参数(A和B)和失败的循环次数(N_F)可以显着影响疲劳寿命,从而导致结果差异。通过使用B = -2模型平滑模型,可以通过不同温度和粘合剂类型去除这种差异。本研究中提出的基于统一的G〜R-R基础分析,导致疲劳寿命较低的标准疲劳模型中的疲劳敏感性较低。统计分析表明,纳米粘土对沥青粘合剂的疲劳寿命没有明显影响。将纳米粘土包含在所有温度下导致相似或略高的疲劳寿命。分析和结果支持使用基于G〜R-R的方法来量化沥青粘合剂的疲劳寿命。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号