In this early study, new cement-bonded bi-composite fibreboard (FB) was made from water hyacinth (WaHy) and waste paper (WP). Ordinary Portland cement (PdCe) used as a binder was mixed with other two additives: gypsum plasters (GyPl) and wood ash (WdAh), in defined proportions to form bonding matrices. The WP and WaHy were pre-treated and a linked process was developed for the mixing and consolidation steps. The FBs produced were based on different proportions of composites, binder, and additives mixed. The FBs produced were made from different proportions of composites, binders, and additives. Improved tensile strength was observed for bi-composite FB from WaHy mixed with WP. In general, FBs having densities in the range of 0.50-0.57 g cm(-3) were compared favourably with the ASTM and ANSI standards (95%), thus making the FBs a potential alternative for building and construction purposes. More elaborate research with advanced analytical techniques is hereby suggested.
机译:在该早期研究中,新的水泥键合双复合纤维板(FB)由水葫芦(Wahy)和废纸(WP)制成。用作粘合剂的普通波特兰水泥(PDCE)与其他两种添加剂:石膏膏药(GYPL)和木灰(WDAH),以确定的比例形成粘合基质。预处理WP和Wahy并为混合和固结步骤开发了联系过程。产生的FBS基于混合的不同比例的复合材料,粘合剂和添加剂。产生的FBS由不同比例的复合材料,粘合剂和添加剂制成。从Wahy与WP混合的Bi-Composite FB观察到改进的拉伸强度。通常,具有0.50-0.57g cm(-3)范围内的密度的FBS与ASTM和ANSI标准(95%)进行比较,从而使FBS成为建筑和施工目的的潜在替代方案。特此建议使用先进的分析技术进行更详细的研究。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号