The Puertollano Integrated Coal Gasification Combined Cycle (IGCC) Power Plant (Spain) fly ash is characterized by a relatively high content of Ga and V, which occurs mainly as Ga_2O_3 and as Ga~(3+) and V~(3+)substituting for Al~(3+) in the Al-Si fly ash glass matrix. Investigations focused on evaluating the potential recovery of Ga and V from these fly ashes. Several NaOH based extraction tests were performed on the IGCC fly ash, at different temperatures, NaOH/fly ash (NaOH/FA) ratios, NaOH concentrations and extraction times. The optimal Ga extraction conditions was determined as 25 ℃, NaOH 0.7-1 M, NaOH/FA ratio of 5 L/kg and 6 h, attaining Ga extraction yields of 60-86%, equivalent to 197-275 mg of Ga/kg of fly ash. Re-circulation of leachates increased initial Ga concentrations (25-38 mg/L) to 188-215 mg/L, while reducing both content of impurities and NaOH consumption. Carbonation of concentrated Ga leachate demonstrated that 99% of the bulk Ga content in the leachate precipitates at pH 7.4. At pH 10.5 significant proportions of impurities, mainly Al (91%), co-precipitate while >98% of the bulk Ga remains in solution. A second carbonation of the remaining solution (at pH 7.5) recovers the 98.8% of the bulk Ga. Re-dissolution (at pH 0) of the precipitate increases Ga purity from 7 to 30%, this being a suitable Ga end product for further purification by electrolysis. This method produces higher recovery efficiency than currently applied for Ga on an industrial scale. In contrast, low V extraction yields (<64%) were obtained even when using extreme alkaline extraction conditions, which given the current marked price of this element, limits considerably the feasibility of V recovery from IGCC fly ash.
机译:Puertollano整体煤气化联合循环(IGCC)电厂(西班牙)飞灰的特点是Ga和V含量相对较高,主要以Ga_2O_3以及Ga〜(3+)和V〜(3+)替代铝粉煤灰玻璃基体中的Al〜(3+)。研究集中于评估这些粉煤灰中Ga和V的潜在回收率。在不同温度,NaOH /粉煤灰(NaOH / FA)比,NaOH浓度和萃取时间下,对IGCC粉煤灰进行了几种基于NaOH的萃取测试。确定了最佳的Ga提取条件为25℃,NaOH 0.7-1 M,NaOH / FA比为5 L / kg和6 h,Ga的提取率为60-86%,相当于197-275 mg Ga / kg粉煤灰。渗滤液的再循环将初始Ga浓度(25-38 mg / L)增加到188-215 mg / L,同时减少了杂质含量和NaOH消耗。浓缩Ga渗滤液的碳酸化表明,在pH 7.4时,渗滤液中99%的整体Ga含量会沉淀。在pH 10.5时,大部分杂质(主要是Al(91%))会共沉淀,而大于98%的Ga残留在溶液中。残留溶液的第二次碳酸化处理(在pH 7.5时)回收了98.8%的Ga。沉淀物的重新溶解(pH在0时)使Ga纯度从7%提高到30%,这是适合进一步生产的Ga终产物电解提纯。该方法产生的回收效率比目前工业规模的Ga高。相比之下,即使使用极端的碱性提取条件,仍可获得较低的V提取率(<64%),考虑到该元素目前的标价,这极大地限制了从IGCC飞灰回收V的可行性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号