In this study, the combination of electric arc smelting and slag refining was employed to produce high purity silicon from Carbonized rice husk (CRH) and silica sand. CaO-SiO2-CaF2 were selected as the slagging agents. Firstly, the CRH was mixed with silica sand and slagging agents. Secondly, the mixed raw materials were pelletized and then melted in an experimental electric arc furnace. Thirdly, the cooling graphite crucible was dissected and divided into four parts, i.e., the loose granular zone, skull zone, cavity zone and product zone. Samples were taken from these four parts and analyzed to study the silicon producing mechanism. It was found that the silicon was produced mainly in the skull zone, and silicon with a purity of 96.97% was obtained at the product zone. By adding slagging agents during the smelting process, the impurities in silicon, i.e., Fe, Al and P were reduced thoroughly from 2.06%, 1.33%, 0.09% to 1.04%, 0.08%, and 0.04%, respectively. The results indicate that adding slagging agents CaO-SiO2-CaF2 can remove the impurities effectively from silicon. After acid leaching, the purity of the silicon can reach up to 99.9%.
机译:在这项研究中,电弧熔炼和炉渣精炼相结合被用来从碳化稻壳(CRH)和硅砂生产高纯度硅。选择CaO-SiO2-CaF2作为造渣剂。首先,将CRH与硅砂和造渣剂混合。其次,将混合的原料造粒,然后在实验电弧炉中熔化。第三,将冷却的石墨坩埚切开并分成四个部分,即松散的颗粒区,头骨区,空腔区和产品区。从这四个部分取样并进行分析以研究硅的产生机理。发现硅主要在头骨区域产生,并且在产物区域获得纯度为96.97%的硅。通过在冶炼过程中加入造渣剂,硅中的杂质,即铁,铝和磷分别从2.06%,1.33%,0.09%分别减少至1.04%,0.08%和0.04%。结果表明,添加造渣剂CaO-SiO2-CaF2可以有效地去除硅中的杂质。酸浸后,硅的纯度可达到99.9%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号