Detoxification of spent cathode carbon blocks from aluminum smelters by joint controlling temperature-vacuum process

机译:通过联合控制温度-真空过程对铝冶炼厂废阴极碳块进行解毒

获取原文
获取原文并翻译 | 示例
           

摘要

The spent cathode carbon block (SCCB) from aluminum reduction cells is considered to be a hazardous material due to containing a large amount of soluble fluoride salts and toxic cyanides. The serious environment pollution and ecological destruction will be caused by being openpiled or buried of SCCB. A joint temperature-vacuum controlling process for treating SCCB is proposed in this paper. The thermodynamic analysis by FactSage 7.0, series of experimental investigation, and characteristics tests on the product materials by SEM and XRD were carried out. The factors including temperature, vacuum pressure and retention time that influence the SCCB's detoxification effects were comprehensively investigated and discussed in detail. It was found out that the soluble fluoride content can be reduced to a level of 3.5 mg.L-1 while cyanide is completely decomposed. A fixed carbon content of 97.89% in the treated materials is obtained under the optimum temperature and vacuum controlling conditions. (C) 2019 Elsevier Ltd. All rights reserved.
机译:由于铝还原池中的废阴极碳块(SCCB)含有大量可溶性氟化物盐和有毒氰化物,因此被认为是有害物质。 SCCB的公开堆放或掩埋会造成严重的环境污染和生态破坏。提出了一种联合处理SCCB的温度-真空控制方法。进行了FactSage 7.0的热力学分析,一系列的实验研究以及通过SEM和XRD对产品材料进行的特性测试。深入研究了温度,真空压力和停留时间等因素对SCCB排毒效果的影响。已经发现,当氰化物完全分解时,可溶的氟化物含量可以降低到3.5mg.L-1。在最佳温度和真空控制条件下,处理过的材料中的固定碳含量为97.89%。 (C)2019 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号