The solvent extraction of copper and zinc from the bioleaching solutions of low-grade sulfide ores with LIX984 and D2EHPA was investigated. The influences of extractant content, aqueous pH value, phase ratio and equilibration time on metals extraction were studied. The results show that LIX984 has a higher selectivity for copper than for iron, zinc and other metals, and has the copper extraction rate above 97%, while the zinc and iron extraction rate is less than 1.6% respectively. Zinc extraction is carried out following the copper extraction from the raffinate. The zinc extraction with di(2-ethylhexyl) phosphoric acid(D2EHPA) is low due to its poor cation exchange. A sodium salt of D2EHPA is used and the zinc extraction rate is enhanced to above 98%. Though iron ( Ⅲ ) is strongly extracted before the extraction of zinc by D2EHPA, it is difficult to strip iron from the organic phase by sulfuric acid. The zinc stripping rate is above 99% with 100 g/L sulfuric acid, while that of iron is 0.16%. Hence, the separation of zinc from iron can be achieved by the selective stripping.
机译:研究了使用LIX984和D2EHPA从低品位硫化矿生物浸提溶液中萃取铜和锌的溶剂。研究了萃取剂含量,水溶液pH值,相比和平衡时间对金属萃取的影响。结果表明,LIX984对铜的选择性高于对铁,锌和其他金属的选择性,铜的提取率高于97%,而锌和铁的提取率分别低于1.6%。从提余液中提取铜后,再进行锌提取。二(2-乙基己基)磷酸(D2EHPA)萃取锌的效率低,这是由于其阳离子交换差。使用D2EHPA的钠盐,锌提取率提高到98%以上。尽管在用D2EHPA萃取锌之前,铁(Ⅲ)被强烈萃取,但是很难用硫酸从有机相中汽提铁。用100 g / L的硫酸,锌的汽提率高于99%,而铁的汽提率为0.16%。因此,可以通过选择性汽提来实现锌与铁的分离。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号