Recently, the use of ultrahigh-performance fiber-reinforced-concrete (UHPFRC) closure joints between structural members has increased in accelerated bridge construction (ABC) applications. This paper presents an experimental study to investigate the structural behavior of UHPFRC closure joints between glass-fiber-reinforced-polymer reinforced-concrete (GFRP-RC) bridge-deck slabs. A total of seven full-scale specimens measuring 3,000-mm long x 1,000-mm wide x 225-mm thick were fabricated, comprised of a reference specimen without closure joints and six jointed specimens. The investigated parameters were: (1) the splice lengths (100, 150, and 200 mm with corresponding joint widths of 120, 170, and 220 mm, respectively); and (2) the reinforcement ratio (No. 15 and No. 20 GFRP bars with the same spacing). The specimens were tested up to failure in a cantilever-panel setup under monotonic line loading in which the UHPFRC closure joint was subjected to flexural and shear stresses. The test results are discussed and analyzed in terms of crack pattern, load-deflection response, crack width, GFRP reinforcement, and concrete strains. The test results show that a minimum splice length of 100 mm in 120 mm UHPFRC closure joints yielded adequate strength and performance until failure. The UHPFRC closure joints remained intact without visible cracks and maintained the continuity between the precast slabs.
机译:最近,在加速桥梁建设(ABC)应用中,在结构构件之间使用超高性能纤维混凝土(UHPFRC)封闭接头的情况有所增加。本文提出了一项实验研究,以研究玻璃纤维增​​强聚合物增强混凝土(GFRP-RC)桥面板之间的UHPFRC封闭缝的结构行为。总共制作了七个尺寸为3,000 mm长x 1,000 mm宽x 225 mm厚的满刻度样品,其中包括不带闭合接头的参考样品和六个接头样品。研究的参数为:(1)接头长度(100、150和200 mm,相应的接头宽度分别为120、170和220 mm); (2)增强比(间距相同的15号和20号GFRP钢筋)。在单调线载荷下,在UHPFRC闭合接头承受弯曲应力和剪切应力的悬臂面板设置中,测试样品直至断裂。对测试结果进行了讨论和分析,包括裂缝模式,荷载-挠度响应,裂缝宽度,GFRP加固和混凝土应变。测试结果表明,在120毫米UHPFRC闭合接头中,最小拼接长度为100毫米,可以产生足够的强度和性能,直至失效。 UHPFRC封闭缝保持完整,没有可见的裂纹,并保持了预制板之间的连续性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号