Sodalite (Na_8(AlSiO_4)_6Cl_2) and cancrinite ((Na,K)_6Ca_2(AlSiO_4)_6Cl_4) are environmentally stable, chloride-containing minerals that are a logical waste form option for the mixed alkali chloride salt waste stream that is generated from a proposed electrochemical separations process during nuclear fuel reprocessing. Here, we discuss a low-temperature, solution-based process to make these phases where sodalite particles are produced in the form of a fine powder with particle sizes on the order of 1-10 μm. Due to the small particle size, these powders require additional treatment to form a monolith. In this study, the powders were pressed into pellets and fired to achieve >90% of the theoretical density of sodalite (2.27 × 10~(-3) kg/m~3). The cancrinite structure, identified as the best candidate mineral form in terms of waste loading capacity, was only produced on a limited basis but was converted to sodalite upon firing. Here, we discuss the specifics of the solution-based approach, the chemical durability of select waste forms as well as the steps taken to maximize the chloride-containing phases, decrease chloride loss during pellet firing, and to increase pellet densities.
机译:方钠石(Na_8(AlSiO_4)_6Cl_2)和方钠石((Na,K)_6Ca_2(AlSiO_4)_6Cl_4)是环境稳定的含氯矿物,对于从碱金属生成的混合碱式氯化物盐废物流来说,这是合理的废物形式提出了核燃料后处理过程中的电化学分离工艺。在这里,我们讨论了一种基于溶液的低温工艺,这些工艺在其中以细粉形式生产方钠石颗粒,细粉的粒径约为1-10μm。由于粒径小,这些粉末需要额外的处理以形成整体。在这项研究中,将粉末压成小丸并烧成方钠石的理论密度(2.27×10〜(-3)kg / m〜3)> 90%。在废物装载量方面被确定为最佳候选矿物形式的铅锌矿结构仅在有限的基础上生产,但在烧成后转变为方钠石。在这里,我们讨论了基于溶液的方法的详细信息,选定废物形式的化学耐久性以及为使含氯相最大化,减少丸粒焙烧过程中的氯离子损失并提高丸粒密度而采取的步骤。

著录项

  • 来源
    《Journal of the American Ceramic Society》 |2012年第10期|p.3115-3123|共9页
  • 作者单位

    Pacific Northwest National Laboratory, Richland, Washington 99352;

    Pacific Northwest National Laboratory, Richland, Washington 99352;

    Pacific Northwest National Laboratory, Richland, Washington 99352;

    Pacific Northwest National Laboratory, Richland, Washington 99352;

    Pacific Northwest National Laboratory, Richland, Washington 99352;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);美国《生物学医学文摘》(MEDLINE);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

  • 入库时间 2022-08-17 13:38:55

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号