首页> 外文期刊>ISIJ international >Dynamic and Isothermal Reduction Swelling Behaviour of Olivine and Acid Iron Ore Pellets under Simulated Blast Furnace Shaft Conditions
【24h】

Dynamic and Isothermal Reduction Swelling Behaviour of Olivine and Acid Iron Ore Pellets under Simulated Blast Furnace Shaft Conditions

机译:模拟高炉竖井条件下橄榄石和酸性铁矿石球团的动态等温还原溶胀行为

获取原文
获取原文并翻译 | 示例
       

摘要

Pellet swelling has been widely studied, being simultaneous with reduction reactions and common in the operation of blast furnaces. A tube furnace equipped with a camera recording system was used here to study the dynamic and isothermal reduction swelling behaviour of olivine and acid pellets under simulated BF shaft conditions. The olivine pellets were magnetically separated into three fractions, containing low, medium and high amounts of magnetite in the core. The divalent iron (FeO) content of these fractions was 0.1 wt-%, 0.2 wt-% and 2.9 wt-%, respectively. Pellets with a large magnetite nucleus were observed to encompass numerous cracks, which was reflected in a poor LTD test value, while SiO_2-rich reference pellets with a different slag chemistry had more restrained swelling and cracking behaviour in dynamic reduction. Swelling in the olivine pellets was associated with cracking at the boundary between the original magnetite nucleus and the hematite shell. The dynamic reduction swelling test results showed lower reduction swelling indices (max 17% in volume) than under isothermal conditions (max 51% in volume), in which case the pellets were suddenly exposed to a strongly reducing atmosphere. It is thus suggested that the reduction swelling behaviour of iron ore pellets should preferably be studied dynamically under simulated blast furnace conditions in order to achieve a realistic understanding of their swelling behaviour in a blast furnace.
机译:球团溶胀已被广泛研究,与还原反应同时进行,并且在高炉操作中很常见。在这里,使用配有摄像机记​​录系统的管式炉来研究在模拟高炉竖井条件下橄榄石和酸丸的动态和等温还原溶胀行为。将橄榄石颗粒磁分离成三个部分,堆芯中含有低,中和大量磁铁矿。这些馏分的二价铁(FeO)含量分别为0.1重量%,0.2重量%和2.9重量%。观察到具有大磁铁矿核的球团包含许多裂纹,这反映在不良的LTD测试值上,而具有不同炉渣化学性质的富含SiO_2的参考球团在动态还原中具有更大的溶胀和开裂行为。橄榄石球团的膨胀与原始磁铁矿核和赤铁矿壳之间的边界处的开裂有关。动态还原溶胀试验结果显示,还原溶胀指数(最大体积为17%)比等温条件下(最大体积为51%)低,在这种情况下,颗粒突然暴露于强烈还原的气氛中。因此,建议最好在模拟高炉条件下动态研究铁矿石球团的还原溶胀行为,以便对它们在高炉中的溶胀行为有一个现实的了解。

著录项

  • 来源
    《ISIJ international》 |2012年第7期|p.1257-1265|共9页
  • 作者单位

    University of Oulu, Laboratory of Process Metallurgy, PO Box 4300, University of Oulu, FI-90014 Finland;

    Ruukki Metals Oy, Rautaruukintie 155, Raahe, FI-92100 Finland;

    University of Oulu, Laboratory of Process Metallurgy, PO Box 4300, University of Oulu, FI-90014 Finland;

    University of Oulu, Laboratory of Process Metallurgy, PO Box 4300, University of Oulu, FI-90014 Finland;

    Boliden Harjavalta Oy, Teollisuuskatu 1, Harjavalta, FI-29200 Finland;

    Ruukki Metals Oy, Rautaruukintie 155, Raahe, FI-92100 Finland;

    University of Oulu, Laboratory of Process Metallurgy, PO Box 4300, University of Oulu, FI-90014 Finland;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);美国《生物学医学文摘》(MEDLINE);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    olivine pellet; acid pellet; reduction; swelling; cracking; isothermal condition; non-isothermal condition; blastfurnace;

    机译:橄榄石颗粒酸丸减少;肿胀;破裂等温条件非等温条件;高炉;