This study focuses on the study of erosion pattern of Blast furnace tuyere which is a copper casted component used for injecting hot air inside the furnace to help in combustion of pulverized coal. As tuyere is operating at high adverse thermal condition; it has provision of two cooling circuits, body and nose separated by solid copper. Identification of the most vulnerable zone in tuyere has been done by scanning used tuyere for which nose cooling circuit does not get failed. This is required to get the actual information regarding erosion pattern as tuyeres changed during shutdown are generally having burnt nose and therefore no use for this study. Scanned model is compared with three dimensional model of original tuyere to find out the erosion pattern. This exercise reveals that the top part of nose front is the weakest zone and hence the maximum material loss is observed at this zone. The reason behind why this particular zone becomes the weakest part is being explained with temperature profile observed in numerical analysis.
机译:这项研究的重点是高炉风口的侵蚀模式,风口是一种铜铸件,用于向炉内注入热空气以帮助燃烧煤粉。由于风口在高温不利条件下运行;它具有两个冷却回路,其主体和机头由实心铜隔开。通过扫描使用过的风口,确保其风口最脆弱区域的使用不会使机头冷却回路失效。这是获得有关侵蚀模式的实际信息所必需的,因为在停机期间更换的风嘴通常会烧伤鼻子,因此在本研究中无用。将扫描模型与原始风口的三维模型进行比较,以找出侵蚀模式。此练习表明,鼻子前部的顶部是最薄弱的区域,因此在该区域观察到最大的材料损失。用数值分析中观察到的温度曲线解释了为什么该特定区域成为最薄弱的部分的原因。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号