This paper is concerned with the influence of water absorption on the time-temperature dependent flexural strength of CFRP laminates. The CFRP laminates were prepared under three conditions of "Dry", "Wet", and "Wet + Dry". The "Dry" laminates were obtained by holding the cured laminates in the oven at 150℃ for 2 hours, the "Wet" laminates were obtained by soaking the "Dry" laminates in hot water at 95℃ for 12, 24 and 48 hours, and the "Wet + Dry" laminates were obtained by dehydrating the "Wet" laminates in the oven at 150℃ for 2 hours. The constant strain rate (CSR) bending tests at various strain rates and temperatures as well as the creep test at various temperatures were carried out for these three kinds of laminates. The time-temperature dependence of flexural CSR strength and creep compliance of these laminates were obtained and the influence of water absorption on these strength and creep compliance were discussed. As results, the master-master curves of CSR strength as well as creep compliance were constructed based on the time-temperature-water absorption superposition principle.
机译:本文关注吸水率对CFRP层压板时温依赖性弯曲强度的影响。 CFRP层压板是在“干”,“湿”和“湿+干”三种条件下制备的。将固化后的层压板在150℃的烤箱中放置2小时,即可获得“干”层压板;将“干燥”层压板在95℃的热水中浸泡12、24和48小时即可获得“湿”层压板,通过将“湿”层压板在烘箱中在150℃下脱水2小时获得“湿+干”层压板。对这三种层压板进行了在各种应变率和温度下的恒定应变率(CSR)弯曲测试以及在各种温度下的蠕变测试。获得了这些层压材料的挠曲CSR强度和蠕变柔度的时间-温度依赖性,并讨论了吸水率对这些强度和蠕变柔度的影响。结果,根据时间-温度-吸水率叠加原理,建立了CSR强度和蠕变柔量的主-主曲线。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号