Influence of Flaws of Wire Rod Surface, Inclusions and Voids on Wire Breaks in Superfine Wire Drawing

机译:极细拉丝中线材表面缺陷,夹杂物和空隙对断线的影响

获取原文
获取原文并翻译 | 示例
           

摘要

By means of the finite element analysis (FEA), this study analyzed wire breaks that occurred in the drawing fine wires containing flaws on the wire surface, inclusion and void. The deformation behavior of an inclusion was examined, in which the inclusion's location is assumed to be on the center axis of the wire, and the cause of wire breaks and their prevention method were clarified. It was found that an inclusion diameter/wire diameter ratio of 0.4 or higher increases the likelihood of wire breaks occurring. When the inclusion is not assumed to be in the center axis of the wire, it was also found that necking and wire breaks appear more frequently. FEA showed that a flaw grows with each processing step, when a small circumferential flaw is placed on the wire rod surface, and eventually becomes a surface defect, which is called a check mark in practice.
机译:通过有限元分析(FEA),该研究分析了在细线中出现的断线,细线中包含表面缺陷,夹杂物和空隙。研究了夹杂物的变形行为,假设夹杂物的位置位于金属丝的中心轴上,并阐明了断线的原因及其预防方法。发现夹杂物直径/线径比为0.4以上会增加发生断线的可能性。当不认为夹杂物位于焊丝的中心轴时,还发现颈缩和断丝的出现频率更高。 FEA表明,当在线材表面上放置一个小的圆周缺陷时,缺陷会随着每个加工步骤而增长,并最终成为表面缺陷,在实践中称为检查标记。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号