Titanium/zirconium diboride cermet coatings were deposited at different laser scan speeds on Ti-6Al-4V alloy using laser cladding technique. Microhardness of the coatings was compared with the microhardness of the substrate, while the microstructural morphologies of coatings were evaluated via scanning electron microscope with energy dispersive spectroscopy. In addition, resultant grain sizes of the coatings were observed and phases formed within the coatings were also examined. The microhardness of the coatings was seen to be four times harder than the substrate. Scanning electron microscopic images exhibited a refinement in grain size and the development of distinct microstructural features. X-ray diffraction patterns showed significant hard phases such as Al_2Zr and Ti_3B_4 which may be responsible for the sky-rocketed microhardness values of the coatings. This study proffers profound insight on the influence of laser scan speed, during deposition, on the microhardness and microstructural morphology of titanium/zirconium diboride cermet coatings.
机译:使用激光熔覆技术以不同的激光扫描速度在钛-6Al-4V合金上沉积钛/二硼化锆金属陶瓷涂层。将涂层的显微硬度与基材的显微硬度进行比较,同时通过具有能谱的扫描电子显微镜评估涂层的显微组织形态。另外,观察到涂层的最终晶粒尺寸,并且还检查了涂层内形成的相。可以看出涂层的显微硬度是底材的四倍。扫描电子显微镜图像显示出晶粒尺寸的细化和独特的微结构特征的发展。 X射线衍射图谱显示出明显的硬质相,例如Al_2Zr和Ti_3B_4,这可能是涂层的超高硬度值的原因。这项研究对沉积期间激光扫描速度对钛/二硼化锆金属陶瓷涂层的显微硬度和显微组织形态的影响提供了深刻的见解。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号