Sm/sub 2/(Co,Fe,Cu,Zr)/sub 17/ magnets with higher Fe content

机译:Sm / sub 2 /(Co,Fe,Cu,Zr)/ sub 17 /具有较高Fe含量的磁体

获取原文
获取原文并翻译 | 示例
       

摘要

The magnetic properties of Sm/sub 2/(Co,Fe,Cu,Zr)/sub 17/ magnets were improved by increasing the Fe content without raising the Zr content. With increasing Fe content, the remanence rises monotonically while the intrinsic coercive force drops sharply for 0.27>v>0.29 and then increases for 0.30>v>0.33 in Sm(Co/sub bal/Fe/sub v/Cu/sub 0.056/Zr/sub 0.02/)/sub 7.546/. For the nominal composition Sm(Co/sub 0.612/Fe/sub 0.316/Cu/sub 0.052/Zr/sub 0.02/)/sub 7.73/, most magnets developed (BH)/sub max/=31-33 MGOe while some reached 33-34 MGOe. Still higher Fe contents may result in further improvement of Sm/sub 2/TM/sub 17/ magnets.
机译:Sm / sub 2 /(Co,Fe,Cu,Zr)/ sub 17 /磁体的磁性能通过增加Fe含量而不增加Zr含量而得到改善。随着Fe含量的增加,剩磁剩磁单调上升,而固有矫顽力在Sm中以0.27> v> 0.29急剧下降,然后以0.30> v> 0.33的Sm(Co / sub bal / Fe / sub v / Cu / sub 0.056 / Zr增大) / sub 0.02 /)/ sub 7.546 /。对于标称成分Sm(Co / sub 0.612 / Fe / sub 0.316 / Cu / sub 0.052 / Zr / sub 0.02 /)/ sub 7.73 /,大多数磁体(BH)/ sub max / = 31-33 MGOe出现了,有些达到了33-34 MGOe。更高的Fe含量可导致Sm / sub 2 / TM / sub 17 /磁体的进一步改进。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号