Sodium sulphite pulping of Scots pine chips in the initial pH range of 7.5-9 was investigated at 180 degrees C and 165 degrees C (for 120-240 min), using chemical charges between 25 and 50% and anthraquinone (AQ) charges 0-0.2%. As a result, pulps with yields of 52-73% and kappa numbers of 35-106 were produced. Delignification was accelerated by higher Na2SO3 charges and temperatures, and by AQ addition, whereas the effect of initial pH was negligible. The high pulp yields at a given kappa number were attributable to high retention of hemicelluloses, especially that of galactoglucomannan. The relatively low viscosities of pulps were apparently caused by depolymerisation of cellulose by sulphite. The sulphonic acid groups in the pulps correlated well with the residual lignin content, although some sulphonation of polysaccharides may also be possible. The results indicate that pulping of softwood in buffer-free (without Na2CO3 and/or NaOH) sodium sulphite liquor may result in pulps with tailored characteristics.
机译:在180℃和165℃(120-240分钟)内,使用25%至50%的化学电荷和蒽醌(AQ)电荷0- 0.2%。结果,制得的果肉的产率为52-73%,卡伯值为35-106。较高的Na2SO3电荷和温度以及添加AQ可以加速去木质素作用,而初始pH的影响可忽略不计。在给定的κ值下,纸浆的高产量归因于半纤维素,尤其是半乳葡甘露聚糖的高保留率。纸浆相对较低的粘度显然是由于亚硫酸盐使纤维素解聚而引起的。纸浆中的磺酸基团与残留的木质素含量密切相关,尽管多糖的某些磺化作用也是可能的。结果表明,在无缓冲液(不含Na2CO3和/或NaOH)的亚硫酸钠溶液中打浆软木可能会产生具有定制特征的纸浆。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号