Column leaching experiments were used to determine the effects of an iron-rich hardpan layer, on the rate of tailings oxidation and the composition of leachate waters, from the Renison Bell tailings dams in western Tasmania, Australia. One-meter-long PVC columns, filled with tailings, cover material (Cassiterite Flotation Tailings) and hardpan samples from the tailings dams, were leached over a period of 14 weeks. Under dry cover conditions, when hardpan was present, the solute loads peaked at 21-49 days (Fe at 2,294 ppm and SO_4~(2-) at 4,700 ppm), and stabilised at much lower concentrations after 9 weeks. In contrast, the solute loads steadily increased over time in the column where hardpan was absent (SO_4~(2-) from 1,800 to 3,100 ppm, and Fe from 407 to 1,692 ppm). Under saturated cover conditions, the solute concentrations in the leachate also increased with time (SO_4~(2-) from 1,900 to 17,000 ppm, and Fe from 480 to 8,500 ppm). The presence of a hardpan layer between the reactive tailings and cover material has been found to improve leachate water chemistry and lessen the rate of sulphide oxidation.
机译:柱浸实验用于确定澳大利亚塔斯马尼亚州西部雷尼森·贝尔尾矿坝的富铁硬壳层对尾矿氧化率和渗滤液水成分的影响。一米长的PVC柱浸有尾矿,覆盖材料(锡石浮选尾矿)和来自尾矿坝的硬盘样品,历时14周。在干覆盖条件下,当存在硬盘时,溶质负荷在21-49天达到峰值(Fe为2,294 ppm,SO_4〜(2-)为4,700 ppm),并在9周后稳定在更低的浓度。相反,在没有硬盘的色谱柱中,溶质载荷随时间稳定增加(SO_4〜(2-)从1,800 ppm到3,100 ppm,铁从407到1,692 ppm)。在饱和覆盖条件下,渗滤液中的溶质浓度也随时间增加(SO_4〜(2-)从1,900 ppm到17,000 ppm,Fe从480 ppm到8,500 ppm)。已经发现,在反应性尾矿和覆盖材料之间存在硬质涂层,可改善渗滤液水的化学性质并降低硫化物的氧化速率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号