A method for detecting the transition from corona from water droplets to dry-band arcing on silicone rubber insulators

机译:一种检测硅橡胶绝缘子从水滴电晕到干带电弧的过渡方法

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

The paper presents an investigation on the use of partial discharge (PD) as a means to study the development of leakage current (LC) on silicone rubber insulators in a salt-fog chamber. Simultaneous measurements of LC and PD on dead-end type silicone rubber insulators exposed to different combinations of electrical stress and salt-fog salinity are performed. The results show that for an electrical stress of 33 V/mm applied to the insulator, the average LC experiences gradual changes and reaches a critical level (around 1 mA) where dry-band arcing is observed after 20 minutes at 2300 /spl mu/S/cm, and after 25 minutes at 1800 /spl mu/S/cm. The corresponding PD levels reach hundreds of pC after 15 minutes at 2300 /spl mu/S/cm, and after 20 minutes at 1800 /spl mu/S/cm. For a salinity corresponding to 1800 /spl mu/S/cm and stress of 26 V/mm, the LC changes much more gradually and reaches the critical level only after approximately 60 minutes. The corresponding PD reaches hundreds of pC after 30 minutes and more than 1500 pC after 60 minutes. Pattern recognition techniques have been applied to investigate the transition from corona to dry-band arcing. The features extracted from the maximum and mean apparent charge trends are found to be useful to cluster and classify the two phenomena. Simultaneous visual observations of the discharges on the insulator surface support the results. The investigation, therefore, shows that PD is a sensitive method for detecting the transition from corona from water droplets to dry-band arcing and an alternative method for studying the early aging stage of silicone rubber insulators.
机译:本文介绍了使用局部放电(PD)作为研究盐雾室内硅橡胶绝缘子泄漏电流(LC)的方法的研究。在暴露于电应力和盐雾盐度的不同组合的终端型硅橡胶绝缘子上,同时测量LC和PD。结果表明,对于施加到绝缘子上的33 V / mm的电应力,平均LC会经历逐渐变化并达到临界水平(大约1 mA),在20分钟后以2300 / spl mu /的速度观察到干带电弧S / cm,并在1800 / spl mu / S / cm 25分钟后。相应的PD水平在2300 / spl mu / S / cm下15分钟后和在1800 / spl mu / S / cm下20分钟后达到数百pC。对于对应于1800 / spl mu / S / cm的盐度和26 V / mm的应力,LC仅在大约60分钟后才会逐渐变化并达到临界水平。相应的PD在30分钟后达到数百pC,在60分钟后达到1500 pC以上。模式识别技术已应用于研究从电晕到干带电弧的过渡。发现从最大和平均视在电荷趋势中提取的特征有助于对这两种现象进行聚类和分类。对绝缘子表面上的放电进行同时的目视观察可以证明结果。因此,研究表明,PD是检测从水滴电晕到干带电弧的过渡的灵敏方法,并且是研究硅橡胶绝缘子早期老化阶段的替代方法。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号