The biodegradable poly(butylene adipate‐co‐terephthalate) (PBAT) polymer was synthesized via one pot synthesis technique using adipic acid and butanediol. The polymerization of synthesized sample was confirmed using FTIR, NMR, and TGA analysis. The PBAT/ATO films were fabricated via spray coating technique utilizing various concentrations of ATO nanoparticles in PBAT polymer solution and optimized the film quality through optical (NIR) and surface analysis. The polymer film having 7 wt % of ATO in PBAT showed good transparency in the UV, visible light and shown approximately 41% absorption in the near infrared region. Moreover, the 7 wt % ATO based polymer film exhibited low surface roughness and uniform coating over the substrate. In addition, near infrared absorbing efficiency of PBAT/ATO composite film in outdoor was demonstrated by constructing a PBAT/ATO (7 wt %)/vinyl greenhouse and the temperature differences were comparatively studied with a bare vinyl green house.
机译:通过使用己二酸和丁二醇通过一种罐合成技术合成可生物降解的聚(丁二酸酯 - 共 - 对苯二甲酸酯)(PBAT)聚合物。使用FTIR,NMR和TGA分析确认合成样品的聚合。通过PBAT聚合物溶液中的各种浓度的ATO纳米颗粒,通过喷涂技术制造PBAT / ATO薄膜,并通过光学(NIR)和表面分析优化薄膜质量。在PBAT中具有7wt%的ATO的聚合物膜在UV,可见光下显示出良好的透明性,并且在近红外区域中显示了大约41%的吸收。此外,7wt%的AtO基聚合物膜在基材上表现出低表面粗糙度和均匀的涂层。此外,通过构建PBAT / ATO(7wt%)/乙烯基温室来证明室外PBAT / ATO复合薄膜的近红外吸收效率,并用裸乙烯基绿房相对较好地研究了温度差异。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号