The purpose of this study was to select and propose an applicable method for extracting lead from sphalerite concentrate direct leaching residue. A large number of experiments were conducted to extract lead from sphalerite concentrate direct leaching residue by hydrochloric acid and sodium chloride solution as leachates. The main optimum parameters were determined, such as a liquid-solid ratio of 17.5-1, a reaction temperature of 85?C, an initial hydrochloric acid concentration of 1.3 mol/L, an initial sodium chloride concentration of 300 g/L, and a reaction time of 60 min. Ninety-five percent of the zinc, 96.0% of the iron, and 93.7% of the lead were extracted into leachate at the optimum conditions. The lead in the leachate was in the form of [PbCl4]2-. After the leachate was purified to remove impurities, it was converted into lead oxalate by sodium oxalate as a precipitant. Finally, lead oxalate was decomposed to obtain lead oxide powders via a high-temperature calcination process.
机译:本研究的目的是选择并提出一种适用的方法,用于从斯巴尔氏素浓缩物直接浸出残留物中提取铅。进行大量实验,以通过盐酸和氯化钠溶液作为浸出物从斯普利特浓缩物直接浸出残留物中提取铅。确定主要的最佳参数,例如液体 - 实体比为17.5-1,反应温度为85〜C,初始盐酸浓度为1.3mol / L,初始氯化钠浓度为300克/升,反应时间为60分钟。在最佳条件下将含量为96.0%的锌,96.0%的铁,93.7%的铅被浸出到渗滤液中。渗滤液中的铅是以[PbCl4] 2-的形式。纯化渗滤液以除去杂质后,将其通过草酸钠作为沉淀剂转化为草酸铅。最后,通过高温煅烧方法分解铅草酸以获得氧化铅粉末。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号