Characterization data of reference industrial polycarboxylate superplasticizers used within Priority Program DFG SPP 2005 “Opus Fluidum Futurum - Rheology of reactive, multiscale, multiphase construction materials”

机译:优先程序中使用的参考产业多羧酸酯超塑性体的表征数据DFG SPP 2005“Opus Flultum Futurum - 反应性,多尺度,多相建筑材料”

获取原文
           

摘要

Two industrial polycarboxylate superplasticizer samples have been selected to be used within the Priority Program 2005 of the German Research Foundation (DFG SPP 2005). The PCE polymers were characterized via Size Exclusion Chromatography (SEC) to determine their molar masses (Mw, Mn), the polydispersity index (PDI) and the conversion rate which indicates the incorporation of the macromonomer into the polymer. The anionic charge amount of the PCE samples was assessed via charge titration employing a cationic polymer. Furthermore, the cement dispersing properties of the PCE polymers were captured via 'mini slump' tests so as to assess their ability to fluidize CEM I 42.5 R and CEM III/A 42.5 N samples, respectively. Also, interaction between the PCEs and the surface of the cements was investigated via adsorption and zeta potential measurements of aqueous cement suspensions. The results shall be used for the ongoing research within the Priority Program.
机译:已选择两个工业多元羧酸盐超塑化剂样品以在德国研究基金会的优先计划2005中使用(DFG SPP 2005)。通过尺寸排阻色谱(SEC)表征PCE聚合物以确定其摩尔质量(MW,Mn),多分散性指数(PDI)和转化率,表示将大分子单体掺入聚合物中。通过采用阳离子聚合物的电荷滴定来评估PCE样品的阴离子电荷量。此外,通过“迷你坍落度”测试捕获PCE聚合物的水泥分散性能,以便分别评估其流化CEM I 42.5 R和CEM III / A 42.5n样品的能力。此外,通过吸附和Zeta电位测量来研究PCE与水泥表面之间的相互作用,然后对水泥液悬浮液进行研究。结果应用于优先计划中正在进行的研究。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号