Photocatalytic degradation of methylene blue under natural sunlight using iron titanate nanoparticles prepared by a modified sol–gel method

机译:用经修饰的溶胶 - 凝胶法制备的铁钛酸盐纳米粒子在自然阳光下的亚甲基蓝色的光催化降解

获取原文
           

摘要

The aim of this work was to synthesize semiconducting oxide nanoparticles using a simple method with low production cost to be applied in natural sunlight for photocatalytic degradation of pollutants in waste water. Iron titanate (Fe 2 TiO 5 ) nanoparticles with an orthorhombic structure were successfully synthesized using a modified sol–gel method and calcination at 750°C. The as-prepared Fe 2 TiO 5 nanoparticles exhibited a moderate specific surface area. The mesoporous Fe 2 TiO 5 nanoparticles possessed strong absorption in the visible-light region and the band gap was estimated to be around 2.16 eV. The photocatalytic activity was evaluated by the degradation of methylene blue under natural sunlight. The effect of parameters such as the amount of catalyst, initial concentration of the dye and pH of the dye solution on the removal efficiency of methylene blue was investigated. Fe 2 TiO 5 showed high degradation efficiency in a strong alkaline medium that can be the result of the facilitated formation of OH radicals due to an increased concentration of hydroxyl ions.
机译:该作品的目的是使用一种简单的方法合成半导体氧化物纳米颗粒,其具有低生产成本的待应用于废水中污染物的光催化降解的自然阳光。使用改性的溶胶 - 凝胶法和750℃的煅烧成功地合成了钛酸钛(Fe 2 TiO 5)纳米颗粒,并在750℃下进行煅烧。制备的Fe 2 TiO 5纳米颗粒表现出适度的比表面积。中孔Fe 2 TiO 5纳米颗粒在可见光区域中具有强烈吸收,估计带隙约为2.16eV。通过自然阳光下的亚甲蓝的降解评估光催化活性。研究了参数的影响,例如催化剂的量,染料初始浓度和染料溶液的pH值对亚甲基蓝的去除效率进行研究。 Fe 2 TiO 5在强碱性介质中显示出高的降解效率,这是由于羟基浓度增加,可以是OH基团的促进形成的结果。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号