For release-liner preparation, coating stabilization of the silicone layer on base paper often requires pre- and post-treatment. In this study, we used atmospheric pressure diffuse coplanar surface barrier discharge in roll-to-roll configuration. The results of prepared coating showed that the A4 size clay-coated paper sprayed with silicone oil (0.25–0.50 mL) gradually decreased the tape peeling force (180°) with prolonged and repeated air plasma post-treatment. Best results showing increased hydrophobicity and significantly enhanced release factor of the coating were obtained after the plasma treatment in a nitrogen atmosphere. The silicone coating on the clay-coated paper reduced the reference release force from 5.5 N/cm to less than 1.5 N/cm after the repeated silicone spraying and short nitrogen plasma post-treatment. The results of X-ray photoelectron spectroscopy and scanning electron microscopy indicate silicone curing by plasma post-treatment and pore-closing of base paper without changes of the bulk material. The aging test lasting 3 months revealed the stability of the prepared coating.
机译:对于剥离衬垫制剂,在基纸上的硅氧烷层的涂层稳定通常需要预处理和后处理。在这项研究中,我们在卷卷构造中使用了大气压漫射共面的表面屏障放电。制备涂层的结果表明,用硅油(0.25-0.50mL)喷涂的A4尺寸粘土涂布纸慢慢地降低胶带剥离力(180°),延长和重复的空气血浆后处理。在氮气氛中的等离子体处理之后,获得了显示出增加疏水性和显着增强释放因子的最佳结果。在重复的硅氧烷喷涂和短氮血浆后处理后,粘土涂布纸上的有机硅涂层从5.5n / cm降低至小于1.5n / cm的基准释放力。 X射线光电子能谱和扫描电子显微镜的结果表明,通过血浆后处理和孔隙闭合的硅氧烷固化而不改变散装材料。持续3个月的老化试验显示制备涂层的稳定性。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号