摘要

The present work shows the temperature dependence of the Raman spectra of two conjugated polymers: poly[2-methoxy-5-(2-ethylhexyloxy)-1,4-phenylenevinylene] (MEH-PPV) and poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonate) (PEDOT:PSS). In situ resonance Raman spectra of PEDOT from 77 to 423 K at 633 nm and of MEH-PPV from 77 to 473 K at 785 nm suggest that, for both polymers, as the temperature increases there is a decrease in the chain conjugation length. Raman bands of PEDOT assigned to the νsim Cα-Cβ are the most sensitive to temperature while bands due to oxyethylene rings do not show significant shifts in this temperature range. Raman and FT-IR spectra of MEH-PPV recorded above the thermal decomposition temperature provide some insights about the thermal degradation.
机译:本作本作表明,两种共轭聚合物的拉曼光谱的温度依赖性:聚[2-甲氧基-5-(2-乙基己氧基)-1,4-苯基乙烯基](MeH-PPV)和聚(3,4-亚乙二氧基烯) - 聚(苯乙烯磺酸盐)(PEDOT:PSS)。在773nm和77至473k的633nm和meh-ppv的PEDOT的原位共振拉曼光谱在785nm的77至473k中表明,对于两个聚合物,随着温度升高,链缀合长度的降低减少。分配给νSIMCα-Cβ的转型的拉曼带对温度最敏感,而氧乙烯环引起的带在该温度范围内不会显示出显着的换档。 RAMAN和FT-IR光谱录制在热分解温度以上,对热降解提供了一些关于热劣化的见解。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号