Full-scale experimental investigation of deposition and corrosion of pre-protector and 3 rd superheater in a waste incineration plant

机译:垃圾焚烧厂中前置保护器和第三过热器的沉积和腐蚀的大规模实验研究

获取原文
           

摘要

Municipal solid waste (MSW) incineration is widely adopted as a waste management strategy and for the energy production. However, this technology experience grave deposition and corrosion of the boiler tubes due to high chlorine (~1.09wt.%) and alkali metal (Na, K) content in MSW. Little is known about the concentration profile of these corrosive elements in the deposits at different boiler locations. Therefore, a full-scale experimental investigation was conducted to determine the concentration profile of Cl, K, Na, S, and Ca in the deposits at pre-protector and compare with those at 3rd superheater during MSW combustion at a 36 MWe waste incineration plant (WIP) in Chengdu, China. The deposit samples were analyzed using wet chemical techniques, scanning electron microscope coupled with energy dispersive spectroscopy (SEM/EDS), and X-ray diffraction (XRD). The concentrations of Na, K, and Cl were high in the deposits at pre-protector while S and Ca concentrations were high on the 3rd superheater. The pre-protector was severely corroded than the 3rd superheater. The governing mechanisms for the deposition and corrosion on these boiler locations were elucidated.
机译:市政固体废物(MSW)焚化被广泛用作废物管理策略并用于能源生产。但是,由于MSW中的高氯(〜1.09wt。%)和碱金属(Na,K)含量,该技术会严重沉积并腐蚀锅炉管。对于这些腐蚀性元素在不同锅炉位置沉积物中的浓度分布知之甚少。因此,进行了一项全面的实验研究,以确定在预保护器处沉积物中Cl,K,Na,S和Ca的浓度分布,并与在36 MWe垃圾焚烧厂的MSW燃烧过程中的第三过热器进行比较。 (WIP)在中国成都。使用湿化学技术,扫描电子显微镜,能量色散光谱法(SEM / EDS)和X射线衍射(XRD)分析沉积物样品。预保护器中沉积物中Na,K和Cl的浓度较高,而第三过热器中S和Ca的浓度较高。预保护器比第三个过热器严重腐蚀。阐明了在这些锅炉位置上沉积和腐蚀的控制机制。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号