Reports of differing failure rates of total hip prostheses made of various metals prompted us to measure the size of metallic and polyethylene particulate debris around failed cemented arthroplasties. We used an isolation method, in which metallic debris was extracted from the tissues, and a non-isolation method of routine preparation for light and electron microscopy. Specimens were taken from 30 cases in which the femoral component was of titanium alloy (10), cobalt-chrome alloy (10), or stainless steel (10). The mean size of metallic particles with the isolation method was 0.8 to 1.0 microns by 1.5 to 1.8 microns. The non-isolation method gave a significantly smaller mean size of 0.3 to 0.4 microns by 0.6 to 0.7 microns. For each technique the particle sizes of the three metals were similar. The mean size of polyethylene particles was 2 to 4 microns by 8 to 13 microns. They were larger in tissue retrieved from failed titanium-alloy implants than from cobalt-chrome and stainless-steel implants. Our results suggest that factors other than the size of the metal particles, such as the constituents of the alloy, and the amount and speed of generation of debris, may be more important in the failure of hip replacements.
机译:由各种金属制成的整个髋关节假体的失败率不同的报告促使我们测量失败的骨水泥置换术周围的金属和聚乙烯颗粒碎片的大小。我们使用一种从组织中提取金属碎片的隔离方法,以及一种用于光镜和电子显微镜的常规制备方法的非隔离方法。取自30例股骨成分为钛合金(10),钴铬合金(10)或不锈钢(10)的标本。分离方法的金属颗粒的平均尺寸为0.8至1.0微米乘1.5至1.8微米。非隔离方法的平均尺寸大大减小了0.3到0.4微米,减小了0.6到0.7微米。对于每种技术,三种金属的粒径均相似。聚乙烯颗粒的平均尺寸为2到4微米乘8到13微米。从失效的钛合金植入物中获取的组织中,它们的体积要大于从钴铬和不锈钢植入物中获取的组织。我们的结果表明,除了金属颗粒的大小以外,其他因素(例如合金的成分以及碎屑的产生数量和速度)在髋关节置换术失败中可能更为重要。
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号