首页> 外文期刊>MATEC Web of Conferences >Interactions between calcium phosphate and heavy metal ions in aqueous solution
【24h】

Interactions between calcium phosphate and heavy metal ions in aqueous solution

机译:水溶液中磷酸钙与重金属离子的相互作用

获取原文
       

摘要

Synthetic and natural calcium phosphates were tested for removal metallic pollution in aqueous solution. Calcium phosphates with Ca/P ratio between 1,33 and 1,67 are fluently called apatite. They have a strong capacity to immobilize metallic ions when they are brought into contact with aqueous solutions. Ca2+ ions can substituted completely or partly by cations such as metallic ions (Ni2+; Cu2+; Co2+ and Cd2+). PO43− ions can be replaced by anions such as AsO43−, CO32−, … etc. Sorption of Cu2+ and Ni2+ from aqueous solutions on natural (NA) and synthetic (SA) apatite was investigated in batch mode at 25 ∘C and 40 ∘C and over metal concentration range of 20–800 mg/L. Other experiments of co-precipitation metal-apatite (metal-TCP) were investigated in static mode at 25 ∘C. The results characterization of NA and SA apatite by FTIR, SEM, and ICP confirm their composition and apatitic structure. The results confirm efficiency of these calcium phosphates to decontaminate, by adsorption or co-precipitation, metallic ions such as Ni2+ or Cu2+ present in aqueous solution at concentrations between 20–800 mg/L.
机译:对合成磷酸钙和天然磷酸钙进行了测试,以去除水溶液中的金属污染。 Ca / P比在1.33和1.67之间的磷酸钙被流畅地称为磷灰石。当它们与水溶液接触时,它们具有固定金属离子的强大能力。 Ca2 +离子可被金属离子(Ni2 +,Cu2 +,Co2 +和Cd2 +)完全或部分取代。 PO43-离子可以被诸如AsO43-,CO32-等阴离子代替。在25∘C和40∘C的分批模式下,研究了从水溶液中天然(NA)和合成(SA)磷灰石上吸附Cu2 +和Ni2 +的过程。 C和超过20-800 mg / L的金属浓度范围。在25°C静态模式下研究了共沉淀金属磷灰石(metal-TCP)的其他实验。 FTIR,SEM和ICP对NA和SA磷灰石的表征结果证实了它们的组成和脂溶结构。结果证实了这些磷酸钙通过吸附或共沉淀来净化水溶液中存在的金属离子(例如Ni2 +或Cu2 +)的效率,其浓度在20-800µmg / L之间。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有