Steel slag is a major industrial waste. Because of poor volume stability, its utilization was limited. We adopted polyphosphate modified steel slag and tailings to produce the autoclaved brick. The effects of various factors influencing the performance of brick were investigated, and the results were obtained: forming water 9%, forming pressure 20MPa, curing regime 4(temperature rising, hr)-4(temperature holding at 180°C, hr)-natural cooling (temperature dropping). With the content of modified steel slag in brick increased from 11% to 25%, the content of cement reduced from 7% to 5%, the compressive strength value increased from 11.6MPa to 22.1MPa.
机译:钢渣是主要的工业废料。由于体积稳定性差,因此其利用率受到限制。我们采用聚磷酸盐改性的钢渣和尾渣生产高压灭菌砖。研究了影响砖性能的各种因素的影响,得到的结果为:成型水9%,成型压力20MPa,固化方式4(升温,hr)-4(保持温度180℃,hr)-自然冷却(温度下降)。随着砖中改性钢渣含量从11%增加到25%,水泥含量从7%减少到5%,抗压强度值从11.6MPa增加到22.1MPa。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号