Evaluation of hydrogen embrittlement and temper embrittlement by key curve method in instrumented Charpy test

机译:夏比试验中关键曲线法评价氢脆和回火脆化

获取原文
           

摘要

Instrumented Charpy test was conducted on small sized specimen of 21/4Cr-1Mo steel. In the test the single specimen key curve method was applied to determine the value of fracture toughness for the initiation of crack extension with hydrogen free, KIC, and for hydrogen embrittlement cracking, KIH. Also the tearing modulus as a parameter for resistance to crack extension was determined. The role of these parameters was discussed at an upper shelf temperature and at a transition temperature. Then the key curve method combined with instrumented Charpy test was proven to be used to evaluate not only temper embrittlement but also hydrogen embrittlement.
机译:对21 / 4Cr-1Mo钢的小型试样进行了仪器化的夏比试验。在测试中,采用单试样关键曲线法确定断裂韧性的值,以无氢开始的裂纹扩展(KIC)和氢脆开裂(KIH)的开始。还确定了撕裂模量作为抗裂纹扩展的参数。在上架温度和转变温度下讨论了这些参数的作用。然后证明了关键曲线法与仪器化的夏比试验相结合不仅可用于评估回火脆化,而且还可用于评估氢脆。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号