Objective: This study mainly focused on use of quarry dust on replaced with river sand for making geopolymer bricks and paver blocks. Method: Investigations were done on usage of eco-friendly Geopolymer Concretes in lieu of OPC concrete for producing geopolymer bricks and paver blocks. Fly ash, GGBS, aggregates and pellet form of sodium hydroxide were mixed together, then, distilled water was added to form alkaline condition. After one-day period, sodium silicate solution was mixed with concrete mixtures to prepare geopolymer concrete. The geopolymer concrete specimen were tested against compressive strength, split tensile strength and flexural strength. Findings: GPCC with 50% sand and 50% quarry dust produced excellent compressive strength, flexural strength and split tensile strength. GPC paver block using 75% GGBS and 25% fly ash shows excellent compressive strength. Geopolymer brick using 65% FA&35% GGBS produced good compressive strength. Applications/Improvements: A high volume fly ash based geopolymer concrete (mix proportion of 65, 70, 75 and 80% FA) used for bricks and high volume ground granulated blast furnace slag based geopolymer concrete (mix proportion of 65, 70, 75 and 80% GGBS) used for pavers blocks.
机译:目的:本研究主要集中在使用采石场粉尘代替河砂来制造地聚合物砖和摊铺机砖。方法:进行了有关使用生态友好的地聚合物混凝土代替OPC混凝土来生产地聚合物砖和摊铺机砖的研究。将粉煤灰,GGBS,骨料和氢氧化钠的颗粒形式混合在一起,然后加入蒸馏水以形成碱性条件。在一天的时间之后,将硅酸钠溶液与混凝土混合物混合以制备地聚合物混凝土。测试了地质聚合物混凝土样品的抗压强度,劈裂抗拉强度和抗弯强度。结果:GPCC含50%的沙子和50%的采石场粉尘,具有出色的抗压强度,抗弯强度和抗拉强度。使用75%GGBS和25%粉煤灰的GPC摊铺机块具有出色的抗压强度。使用65%FA和35%GGBS的地聚合物砖可产生良好的抗压强度。应用/改进:用于砖的高粉煤灰基土聚合物混凝土(混合比例为65、70、75和80%FA)和高磨碎矿渣高炉矿渣基土聚合物混凝土(混合比例为65、70、75和75%) 80%GGBS)用于摊铺机块。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号