Preparation of Silver Nanoparticles in Ultrasonic Vibration-Induced Nanodroplets of Isopropyl Alcohol in Combination with Ionic Liquids

机译:超声振动诱导的异丙醇与离子液体结合的纳米液滴中银纳米颗粒的制备

获取原文
           

摘要

Silver nanoparticles (10 nm) were prepared in ultrasonic vibration-induced nanodroplets of isopropyl alcohol (IPA) in combination with hydrophobic room temperature ionic liquids (RTILs). The Ag-precursor used were silver (I) complex, Ag2(ehac)2(eha)2 (ehac = 2-ethylhexylammonium carbamate; eha = 2-ethylhexylamine), in IPA, while 1-butyl-3-methylimidazolium-based ionic liquids bearing SbF6 −, PF6 − and NTf2 − as counter anions were used as RTILs. During sonication for 10-90 min at room temperature, uniform silver nanoparticles with mean sizes of 2 to 8 nm were rapidly synthesized. Transmission electron micrographs also confirmed that silver nanoparticles have a spherical shape and diverse sizes depending on the reaction time (10-90 min).
机译:在超声振动诱导的异丙醇(IPA)的纳米液滴与疏水性室温离子液体(RTIL)的组合中制备银纳米颗粒(<10 nm)。在IPA中使用的银前体是银(I)络合物,Ag2(ehac)2(eha)2(ehac =氨基甲酸2-乙基己基铵; eha = 2-乙基己胺),而基于1-丁基-3-甲基咪唑鎓的离子将带有SbF6-,PF6-和NTf2-作为抗衡阴离子的液体用作RTIL。在室温下超声处理10-90分钟期间,快速合成了平均粒径为2至8 nm的均匀银纳米颗粒。透射电子显微照片还证实,取决于反应时间(10-90分钟),银纳米颗粒具有球形形状和各种尺寸。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号