首页> 外文期刊>Journal of the Ceramic Society of Japan >Preparation of lithium nickel manganese oxide cathode material for 5V-class high-voltage batteries by a microwave heating method
【24h】

Preparation of lithium nickel manganese oxide cathode material for 5V-class high-voltage batteries by a microwave heating method

机译:微波加热法制备5V级高压电池用锂镍锰锰正极材料

获取原文
           

摘要

Lithium nickel manganese oxide cathode material, LiNi0.5Mn1.5O4, was prepared by an improved microwave heating method. Prepared cathode materials were characterized by X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), scanning electron microscope (SEM), and charge–discharge measurements. XRD results indicated that single-phase LiNi0.5Mn1.5O4 powders were obtained under the optimized preparation conditions. SEM investigation demonstrated that the powders had an octahedron shape and a particles size of about 200–300 nm. The obtained LiNi0.5Mn1.5O4 exhibited good electrochemical performance and delivered an initial discharge capacity of 145 mAh g?1 at a current density of 20 mAg?1.
机译:采用改进的微波加热法制备了锂镍锰氧化物正极材料LiNi 0.5 Mn 1.5 O 4 。制备的阴极材料通过X射线衍射(XRD),傅立叶变换红外光谱(FT-IR),扫描电子显微镜(SEM)和充放电测量来表征。 XRD结果表明,在优化的制备条件下获得了单相LiNi 0.5 Mn 1.5 O 4 粉末。 SEM研究表明,这些粉末具有八面体形状,粒径约为200-300 nm。所得的LiNi 0.5 Mn 1.5 O 4 具有良好的电化学性能,初始放电容量为145 mAh g ?1 ,电流密度为20 mAg ?1

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号