A nickel-loaded activated carbon (Ni/AC) composite particle electrode was prepared by electroless deposition with palladium-free pretreatment to improve the electrocatalytic performance of a composite particle electrode in a three-dimensional electrode cell. The preparation conditions of the Ni/AC particle electrode were optimized using the decolorization ratio of methyl orange dye solution as an index. The composite particle electrodes were characterized by scanning electron microscopy, X-ray diffraction, and energy dispersive spectrometry analyses. The electrocatalytic performances of the Ni/AC particle electrode were examined by a series of parameters, including particle electrode dose, sodium sulfate concentration, cell voltage, and electrolysis time. The results were compared with those of conventional activated carbon (AC) particle electrode. These results indicated the feasibility of preparing a Ni/AC composite particle electrode by electroless plating with non-palladium pretreatment. The optimal conditions for preparing the Ni/AC electrode were 40 g L-1 NiSO4·6H2O, 27 g L-1 NaH2PO2·H2O, 50 °C plating temperature, and 20 min plating time. The electrocatalytic performance of Ni/AC electrode was superior to that of AC electrode under the same electrolysis conditions. The rate constant of the Ni/AC electrode electrochemical oxidation of methyl orange was 1.5 times larger than that of AC electrode.
机译:通过无钯预处理的化学沉积法制备了负载镍的活性炭(Ni / AC)复合颗粒电极,以改善复合颗粒电极在三维电极池中的电催化性能。以甲基橙染料溶液的脱色率为指标,优化了Ni / AC颗粒电极的制备条件。通过扫描电子显微镜,X射线衍射和能量色散光谱分析对复合颗粒电极进行了表征。 Ni / AC颗粒电极的电催化性能通过一系列参数进行检查,包括颗粒电极剂量,硫酸钠浓度,电池电压和电解时间。将结果与常规活性炭(AC)颗粒电极的结果进行了比较。这些结果表明通过非钯预处理的化学镀制备Ni / AC复合颗粒电极的可行性。制备Ni / AC电极的最佳条件是40 g L-1 NiSO4·6H2O,27 g L-1 NaH2PO2·H2O,50°C的电镀温度和20分钟的电镀时间。在相同的电解条件下,Ni / AC电极的电催化性能优于AC电极。甲基橙的Ni / AC电极电化学氧化速率常数是AC电极的1.5倍。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号