Evaluation of Impact of Yarn Count and Stitch Length on Pilling, Abrasion, Shrinkage and Tightness Factor of 1 x 1 Rib Cotton Knitted Fabrics

机译:支数和针迹长度对1 x 1罗纹棉针织面料起球,磨损,收缩和紧密度因子的影响评估

获取原文
           

摘要

This study investigates the impact of yarn count and stitch length of 100% cotton knitted fabrics. 1 x 1 ribs structured fabrics were used in this research work. The stitch length 2.50 mm, 2.52 mm, 2.60 mm, 2.70 mm, 2.80 mm and 2.96 mm were used of the yarn count of 26Ne, 28Ne and 36Ne. The areal densities of the grey fabrics were in various amounts. The impacts of yarn count and stitch length were measured concerning pilling resistance, abrasion resistance, and shrinkage and tightness factor. The result showed that the fabric pilling grade decreased while number of cycle increased. Abrasion resistance decreased but length wise shrinkage increased despite the fact that the stitch length increased. The results also exposed that the tightness factor of the fabric increased with the increase of the stitch length in both dyeing and washing state and finished state compared to grey state for the yarn count 26Ne and homogeneous result not found for yarn count 28Ne and 36 Ne.
机译:本研究调查了100%棉针织面料的支数和线迹长度的影响。 1 x 1肋结构的织物用于这项研究工作。使用26Ne,28Ne和36Ne的纱线支数的针迹长度2.50mm,2.52mm,2.60mm,2.70mm,2.80mm和2.96mm。坯布的面密度不同。测量了纱线支数和线迹长度对抗起球性,耐磨性以及收缩率和紧密度因子的影响。结果表明,织物起球等级降低,而循环次数增加。尽管针迹长度增加,但耐磨性降低了,但纵向收缩却增加了。该结果还显示出,与纱线状态26Ne的灰色状态相比,在染色状态和洗涤状态以及最终状态下,织物的紧密度因子均随着针迹长度的增加而增加,而对于纱线28Ne和36Ne而言,其紧密度结果均未发现。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号