AbstractBackground & aim: The most important features of dental materials is physical surface. One of these features is interfacial effect of solid–fluid that evaluated in standard situation with contact angle and the surface tension is directly related to it. This study was aimed to evaluate two mouth-rinse contact angle with difference base on two restorative materials. Method & Material: In this experimental study we has made 15 composites dick, 15 Glass Ionomers) disk with 6mm diameter and 2mm thickness and good surface roughness and used artificial saliva as control group, chlorhexidine and persica mouth-rinse and Contact angle of each instilled drop of liquids on the surface of restorative materials was measured whit profile imaging in the same condition. The obtained data were analyzed by ANOVA and Tukey. Result: the most contact angle was in artificial saliva on composite surface (55.7 ?) and the least of them was chlorhexidine in Glass Ionomer surface (33 ?). Also there was Significant differences between all conditions studied (P0.001), except persica and artificial saliva on the composite (P=0.324). Conclusion: in this study Between two restorative materials, composite (hydrophobic) and glass ionomer (hydrophilic) contact angle of artificial saliva, persica and chlorhexidine on the more hydrophilic material (glass ionomer) is lower and among the solutions used, chlorhexidine contact angle on the both restorative material is less.
机译:摘要背景与目的:牙科材料最重要的特征是物理表面。这些特征之一是固液的界面效应,该效应在标准情况下通过接触角进行评估,表面张力与其直接相关。这项研究旨在评估基于两种修复材料的两种漱口接触角的差异。方法和材料:在本实验研究中,我们制作了15个直径6mm,厚度2mm且表面粗糙度良好的复合材料盘,15个玻璃离子聚合物盘,并以人工唾液为对照组,洗必泰和波斯菊的漱口液和每次滴入的接触角在相同条件下通过轮廓成像测量了修复材料表面上的液体滴。通过ANOVA和Tukey分析获得的数据。结果:最大的接触角是在复合材料表面的人造唾液中(55.7°),而最小的是玻璃离聚物表面的洗必太(33°)。在研究的所有条件之间也存在显着差异(P <0.001),复合材料上的波斯菊和人工唾液除外(P = 0.324)。结论:在这项研究中,在两种修复材料之间,人造唾液的复合(疏水性)和玻璃离聚物(亲水性)接触角,波斯菊和洗必泰在亲水性更高的材料(玻璃离聚物)上更低,并且在使用的溶液中,洗必泰的接触角在两种修复材料都较少。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号