This research is experimental research aimed at to investigate the effect in using retarder onto concrete workability and compressive strength. The sample will be made of concrete cube with uniform size is 15 cm x 15 cm x 15 cm. the total amounts of cube are 96 pieces, each 32 samples for each data groups into 0%, 1%, 2% and 4%, the sample are then kept fresh with various time, 0 minute, 10 minutes, 15 minutes and 20 minutes. The fresh sample’s feasibility and compressive strength will be examined at 7, 14, and 28 days concrete. The result shows workability concrete changing in case retarder addition. The higher retarder concentrations cause either increased slump value or easy-made concrete. The longer fresh concrete are storage will result in decreased in slump value or the concrete is viscous. In concrete with age 7, 14, 28 days, the highest pressure strength is 2%. Additions in 4% retarders are significantly degraded pressure strength. Concrete storage up to 20 minutes does not give significant concrete pressure strength.
机译:这项研究是实验研究,旨在研究使用缓凝剂对混凝土的可加工性和抗压强度的影响。样品将由均匀尺寸为15厘米x 15厘米x 15厘米的混凝土立方体制成。立方体的总量为96件,每个数据组的每个32个样本分为0%,1%,2%和4%,然后在不同的时间,0分钟,10分钟,15分钟和20分钟内保持新鲜。新鲜样品的可行性和抗压强度将在7、14和28天的混凝土中进行检查。结果表明,在添加缓凝剂的情况下,可加工性混凝土发生了变化。较高的缓凝剂浓度会导致坍落度值增加或混凝土易于制造。新鲜混凝土的储存时间越长,其坍落度值降低或混凝土粘稠。在7、14、28天的混凝土中,最高抗压强度为2%。 4%缓凝剂的添加会显着降低耐压强度。长达20分钟的混凝土储存不会产生明显的混凝土抗压强度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号