The influence of silane debonder on the properties of fluff pulp fibers was investigated. The results showed that the burst index and internal bond strength of pulp sheet decreased with the increasing debonder loading. The density and zero-span tensile strength didn’t change significantly when the debonder was added. The absorption capacity of fiber increased with increasing the de-bonder loading and achieved a maximum value of 10.3 g·g-1 when the debonder loading was 2.5%. The relevant mechanism was studied by X-ray Diffraction (XRD), Fourier transform infrared (FT-IR) spectroscopy, and energy dispersive X-ray analysis (EDAX). XRD analysis indicated that the debonder had no great influence on the crystal structure of fiber. FT-IR analysis results showed that it was easier to break the intermolecular hydrogen bond than the intramolecular hydrogen bond with the incorporation of debonder. Therefore, the proportion of intramolecular hydrogen was increased. The EDAX results indicated that the debonder can decrease the binding force of fiber by shielding the hydroxyl groups and preventing the formation of hydrogen bonds.
机译:研究了硅烷脱粘剂对绒毛浆纤维性能的影响。结果表明,纸浆板的破裂指数和内部粘结强度随着脱胶剂负荷的增加而降低。添加脱胶剂后,密度和零跨度拉伸强度没有明显变化。纤维的吸收能力随着脱胶负荷的增加而增加,当脱胶负荷为2.5%时,其吸收最大值达到10.3 g·g-1。通过X射线衍射(XRD),傅立叶变换红外(FT-IR)光谱和能量色散X射线分析(EDAX)研究了相关机理。 XRD分析表明,脱胶剂对纤维的晶体结构影响不大。 FT-IR分析结果表明,通过结合去键合剂,比分子内氢键更容易断裂分子间氢键。因此,分子内氢的比例增加。 EDAX结果表明,该脱粘剂可通过保护羟基并防止氢键的形成而降低纤维的结合力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号